SHANGHAI MICROCRE OPTICS-MECH TECH CO., LTDAbout MICROCRE400-812-7833
TOPICS

Proof strength Rp0.2 interpolation

This entry gives the definition, variables, assumptions and a reproducible example for Proof strength Rp0.2 interpolation. The equation holds only under the stated assumptions.

Derivation

Write inputs and outputs by definition and convert to the unit system required by the equation.

Check dimensional consistency, then judge whether the result is physically plausible.

Common pitfalls

Extrapolating an empirical equation beyond validated materials or conditions

Mixing unit systems without conversion

Assumptions

  • • Inputs are independent and measured as defined
  • • Conditions are stable without unmodelled bias
  • • Units and magnitudes stay within the valid range

Illustrative example

Inputs

Example inputs: Lower stress=350 MPa; Lower strain=0.15 %; Upper stress=365 MPa; Upper strain=0.25 %

Steps

Substitute and keep significant digits.

Result

See the default result in the linked calculator; values are illustrative.

Equation

R_p0.2 = σ₁ + (0.2 − ε₁)/(ε₂ − ε₁) · (σ₂ − σ₁)

Symbols & units

s1Lower stressMPa
e1Lower strain%
s2Upper stressMPa
e2Upper strain%

Proof strength Rp0.2 interpolation →

Related instruments & resources

Links support navigation and do not establish a model’s performance or standards compliance.

Your next research question. Let’s explore.

Tell us about your material, specimen and measurement goal.

Discuss your application ↗
Find your instrument
⌕
Search products, cases, solutions, standards and literature.