Removing sectioning burn from case-depth judgement

Case depth on the same batch differed by 0.1 mm between laboratories; the cause had to be traced to preparation or material.

Industry:Heat treatment and metallographyInstruments:ZXG-100 · XQ-2B · ZMP-2000Z · HVS-1000

The constraint

Fast abrasive cutting creates a white layer and micro-cracks; microhardness there reads high and is easily mistaken for case depth.

Approach

Re-cut with a resin-bonded thin blade and higher coolant flow, prepare side by side with the original and compare hardness at equal depth.

  1. Re-cut at low feed with immediate cooling to avoid tempering
  2. Indent at equal depth on both, compare the two profiles
  3. Judge from the burn-free profile and write it into the procedure

Outcome

The gap closed to under 0.02 mm; cutting parameters became mandatory in the work instruction.

Related instruments

Application scenario files: industry, workpiece type and measurement goals come from routine engineering discussions. Customer names and specific data are anonymized; nothing here is a traceable commercial record or a commitment about any customer's production results.

← All application files

Your next research question. Let’s explore.

Tell us about your material, specimen and measurement goal.

Discuss your application ↗
Find your instrument
⌕
Search products, cases, solutions, standards and literature.