SHANGHAI MICROCRE OPTICS-MECH TECH CO., LTDAbout MICROCRE400-812-7833
APPLICATION FILE / Advanced ceramics

Hot hardness of structural ceramics at 1200 ℃

SiC-alumina composites need hardness at 1200 ℃ for wear-part material selection.

Industry:Advanced ceramicsInstruments:HMAS-HT1200

The constraint

Cracks form around hot indents and are hard to image; heating rate and dwell time strongly affect results.

Approach

Heat in inert atmosphere to the set temperature, indent at an agreed force and dwell, then measure diagonals after cooling and record cracks.

  1. Polish below Ra 0.05 µm, clamp, evacuate and backfill argon
  2. Hold 30 min at 1200 ℃, make three indents with 15 s dwell
  3. Cool in furnace, measure diagonals and note crack length

Outcome

A dataset near 12 GPa at 1200 ℃ was obtained and crack length used as a toughness indicator; conditions entered the incoming specification.

Related instruments

Application scenario files: industry, workpiece type and measurement goals come from routine engineering discussions. Customer names and specific data are anonymized; nothing here is a traceable commercial record or a commitment about any customer's production results.

← All application files

Your next research question. Let’s explore.

Tell us about your material, specimen and measurement goal.

Discuss your application ↗